Laser hot-wire brazing without RCU 5000i

A: Start of brazing

To obtain good wetting to sidewalls in the brazed join, ensure the following:
-
-
Preconditions for laser hot-wire brazing
Points 3., 4. and 5. describe analogue input signals.
Re. Point 3.:
-
-
NOTE!
A clearer overview of the program can be obtained by amalgamating all the signals
into one single command in a sub-program (e.
g. "Start of brazing").
IMPORTANT! Laser hot-wire brazing is a spatter-free process. This means that it is not
absolutely necessary to have an additional fume-extractor. It is sufficient if the crossjet can
be clearly heard working (at an operating pressure of between 0.5 and 1 bar = 7.22 - 14.45
psi).

B: End of brazing

1
2
3
4
5
6
7
8
Focus diameter = Wire diameter + 30%
Torch tilt angle is 35° (trailing)
35 °
+30 %
Welding voltage = welding current x welding circuit resistance
(welding circuit resistance depends on the contact tip and filler metal)
Value is below 10 V (voltage limitation)
"Stop movement of the robot"
Reset "Wire feed"
Reset "Welding ON"
Initialise "Wire retract"
Initialise "Time-lag" (0.2 s)
Reset "Wire retract"
Initialise "Laser OFF"
Reset "Gas test"
Initialise "Gas test"
1
Select operating mode 5 "CC / CV"
2
-
Set operating bit "0" to "1"
-
Set operating bit "1" to "0"
-
Set operating bit "2" to "1"
Welding voltage: Specify "Pulse/dyna-
3
mic correction"
Welding current: Specify "Welding po-
4
wer"
Wire feed speed: Specify "Arc length
5
correction"
Initialise "Welding ON"
6
100 %
Initialise "Wire feed"
7
Wait for current flow signal ("Arc esta-
8
blished")
Initialise "Laser ON"
9
Initialise "Robot start"
10