FinishControl 6500 TS
malfunctIon
Coating material causes "paint
tears
Excessive paint mist (overspray)
Poor spray pattern
Paint in the ventilating hose
The spray pattern deteriorates
during painting
16
AcceSSorIeS And SPAre PArtS
16.1
AcceSSorIeS
order no.
Pos.
desIgnatIon
1
2321 879
StandardSpray spray attachment (yellow) (with 1000 ml container)
Processes all standard paints.
2
2321 877
FineSpray spray attachment (brown) (with 1000 ml container)
Ideal for low-viscosity paints and glazes.
3
2321 880
WallSpray spray attachment (white) (with 1400 ml container)
Designed for processing dispersions.
4
2324 749
Container with cover (1400 ml)
5
Container with cover (1000 ml)
2322 451
cause
•
Too much coating material applied
•
Distance too small
•
Incorrect spray attachment
•
Distance to the object too large
•
Too much coating material applied
•
Amount of air too high
•
Coating substance over-diluted
•
Incorrect spray attachment
•
Paint has been destroyed by
overheating
•
Container was too hot before the
heating process started. The heating
process was not executed correctly.
•
Diaphragm soiled
•
Diaphragm defective
•
Nozzle/air cap is dirty
•
The paint has cooled down too much
correctIon of malfunctIons / accessorIes and sPare Parts
remedy
•
Reduce volume
•
Increase distance
•
Use another spray attachment
•
Reduce distance
•
Reduce volume
•
Reduce volume
•
Reduce degree of dilution
•
Use another spray attachment
•
Reduce temperature setting (adhere to data
sheet provided by manufacturer)
•
Allow container to cool briefly and then reheat
paint
•
Clean the diaphragm (see section 14.2)
•
Replace the diaphragm (see section 14.2)
•
Detach the air cap and clean both parts
(especially the hole in the middle of the air cap)
•
Reheat the paint