GB
D
Problem
Spray jet is
uneven/ not
constant
Coating
material causes
"paint tears"
Too much fog of
coating material
(Overspray)
Width of paint
spray cannot be
adjusted
Poor covering
capacity on the
wall
Coating
material cannot
be atomised
48
48
Cause
•
Coating material in container
running out
•
Nozzle seal worn
•
Air filter heavily soiled
•
Filter clogged at suction hose
•
Too much coating material
applied
•
Viscosity of coating material too
low
•
Distance to the object too large
•
Too much material quantity
•
At a low quantity of material, wide
spray jet selected (black)
•
Adjustment ring is not connected
to the peg on the air cap
•
Air screen is clogged up
•
Spray material is too cold
•
Highly absorbent surface
or paint with poor covering
capacity
•
Distance too large
•
The material quantity and spray
jet do not correspond with each
other
•
Multifunction switch is set to
"Clean"
•
Turbine is defect
W 950 Flexio
W 950 Flexio
Remedy
➞ Refill
➞ Replace
➞ Change
➞ Clean filter
➞ Turn the material volume
setting to the left
Spray excess material on the
wall using the inking roller
➞ Reduce the quantity of
material and apply in several
layers
➞ Reduce distance
➞ Turn the material volume
setting to the left
➞ Switch to narrow jet spray
(white)
➞ Connect adjustment ring
and peg
➞ Disassemble and clean the
spray head
➞ The material you are
spraying should be at room
temperature
➞ Cross spray (Fig. 8)
➞ Closer to the object
➞ Optimise the settings
➞ Set the multifunction switch
to "ON"
➞ Please contact Wagner
Service