1)Do not remove the small amounts of excess Variolink II
before polymerization. Thus, only the excess is affected by
oxygen inhibition and may easily be removed after
polymerization during finishing of the margins.
2)Cover restoration margins with a glycerine gel (e.g. Liquid
Strip) after removal of excess, but before the polymeriza-
tion. Thus, oxygen inhibition can be avoided.
9. Finishing/Polishing
– Remove polymerized excess with a finishing diamond
(grain size below 25 µm), and flexible discs.
– Apply finishing and polishing strips in the proximal
regions.
– Check occlusion and functions and make corrections if
necessary.
– Polish restoration margins with silicone polishers
(Politip-F/-P, Astropol
®
) or discs.
10. Topical fluoride application
Fluoride the tooth after completion of the restoration
(e.g. with Fluor Protector).
Warning:
Avoid contact of Variolink II with skin, mucous membrane,
and eyes. Unpolymerized Variolink II may cause slight
irritations and may lead to a sensitization against
methacrylates.
Storage
– Do not use Variolink II after expiry date.
– Cool storage (2–8 °C/36–46 °F) is indicated for the
catalyst paste.
– Note: Syringes should be closed immediately after use.
Exposure to light causes premature polymerization.
– Shelf life: see expiry date
Keep material out of the reach of children!
For use in dentistry only!
Date information prepared:
05/2003
Manufacturer:
Ivoclar Vivadent AG
FL-9494 Schaan / Liechtenstein
This material has been developed solely for use in dentistry. Processing should be
carried out strictly according to the Instructions for Use. Liability cannot be
accepted for damages resulting from failure to observe the Instructions or the
stipulated area of application. The user is responsible for testing the material for its
suitability and use for any purpose not explicitly stated in the Instructions.
Descriptions and data constitute no warranty of attributes and are not binding.