The welding conditions must be reviewed at the start of each new job. «Test» weld spots must be carried out on metal panels
or sheets similar to the new job being undertaken. Carry our two spot weld with appropriate space in between, in line with the
requirement of the job. Test the strength of the second weld. The test is successful if, when pulling the spot out, the panel breaks
and the centre is extracted. The centre must have a minimum diameter in line with the specifications of the make of the vehicle.
AUTO mode
In order to use this mode, do a blank spot weld (without any sheet/panel between the electrodes),as prompted on the display. Push the button (FIG 2
-11). The message «Do a spot without a load» is displayed on the screen. Push the button again to calibrate. Once the calibration is done, the machine
shows all the settings to zero, and is ready to weld. Close the clamp on the area to weld and weld automatically, without entering any parameters in
the machine. Every 30 spots, a new calibration will be required.
This mode can be used when using all arms except the G7.
NORMAL mode
Push the button
for 2 seconds to return to the AUTO mode.
MANUAL mode
Push the button
for 2 seconds to return to the AUTO mode.
MULTI mode
Push the button
for 2 seconds to return to the AUTO mode.
46
BMW C7502654 - GYSPOT PTI GENIUS
This mode is displayed by default when the machine starts.
This mode is used to weld sheets/panels without having to specify any settings on the screen. The machine
sets the appropriate settings automatically.
This mode determines the welding settings based on the thickness of the sheets/panels and the type of
steel.
The settings that need to be set when using this mode are:
- Thickness of the sheets/panels, with a range between 0.60 mm and 3.00 mm.
When 2 sheets/panels are being welded together, enter the thickness of the thinnest sheet.
When 3 sheets/panels are welded together, use the total cumulated thickness and divide by 2.
- Type of steel (coated steel, HLE/THLE steel, UHLE steel, bore steel (BORON)).
When welding a mix of different types of steel, select the strongest one.
- Reference of the arm used.
This mode is used to select the parameters of the spots by following the instructions of a repair book.
The parameters to set in this mode are:
- Current
- Duration
- Pressure
- Reference of the arm used.
This mode is used to set precisely the thickness and type of steel for each sheet/panel .
The first element (thickness of sheet 1) is selected. The keys up and down are used to select the setting that
needs to be adjusted, where the keys right and left are used to increase or decrease the value. Highlight the
setting that needs to be adjusted.
The settings that need to be set when using this mode are:
- Thickness of the sheets/panels, with a range between 0.60 mm and 2.50 mm.
- Type of steel (coated steel, HLE/THLE steel, UHLE steel, bore steel (BORON)).
When welding a mix of different types of steel, select the strongest one.
- To activate the sheet/panel 3, press the scroll keys (
keys + and - to select the thickness of the sheets/panels.
- Reference of the arm used.
or
) to highlight sheet/panel 3. Then use they
EN