Glue failure: visible separation of the glue from itself,
the coating, or dolly (no coating visible on the dolly face).
Cohesive fracture
(within a layer)
Glue failures typically occur when the glue is improperly mixed or
the coated surface has not been adequately prepared (pg. 4).
The PosiTest AT-A provides an interface to document the nature
of the fracture for each pull-off test (pg. 7). Fracture results are
included in test reports.
The PosiTest AT-A stores 100,000 readings in up to 1,000
batches. Stored measurements can be reviewed on-screen or
accessed via computers, tablets, and smart phones.
New Batch
Closes any currently opened batch and creates a new memory
batch, named using the lowest available number (example: B2).
New batches are date stamped when they are created.
Open
Selects a previously created batch to open and make current.
Dolly
SUBSTRATE
Adhesive fracture
(between layers)

Memory Menu

9
Glue
Glue failure
(coating/glue)

Publicité

Table des Matières
loading

Table des Matières