The stainless steel components do not require special maintenance. The appearance of micro-oxidation, more
frequent in maritime environments subject to salt spray, does not affect the quality and durability of the product. Such
Stainless steel
oxidation is normal. If you need to eliminate these oxidised spots you can use a steel wool or a brush with stainless steel
bristles. The protective chromium oxide film (self-passivation) will be restored naturally just through exposure to air, without
any intervention by the user.
Aluminium
The presence of marks and scratches is considered as a defect only if they are visible at a distance of 2 metres.
Painting
Rev. 1 - 06.2018
CORRADI SRL - USER MANUAL
Non-conformity / defect
If the marks and/or dents are visible at a distance of 2
metres it is considered as a defect.
Orange peel: the surface of the coating film is uneven and
looks like an orange peel.
Blistering: bulges on the surface of the coating film of
various sizes and frequency.
Sagging of the outer layer: irregular accumulations of
paint localised and well defined in the form of shallow,
rounded edges affecting the outer layer.
Flaking - Peeling: the coating film detaches from the
underlying support in the form of small flakes.
Porosity - Pitting: small holes similar to craters or indentations
in the surface of the film, ranging in size from small pin-holes
up to diameters of 1 cm.
Impurities in the outer and inner layers: the paint film has a
rough and uneven surface, easily perceptible to the touch.
Paint chips due to interference: the paint film has damage
and lesions of different depth and extent depending on
the cause.